Obviously it's an essential tool to for Anhydrite prep and and a handy thing to have I have 3 Tbo but I tend to use them a grinders rather than...
It's a bit of a grey area Some manufacturers say you can DPM if it's almost dry but its pointless really as its fast drying and A DPM will slow...
Agree with Mario Definitely looks like an Anhydrite Grinding looks ok as you've removed the top and you can see the aggregate
No
Good stuff ;)
No need to sand smoothing compounds on domestic jobs or at all if possible Your just making more work for your self
I haven't no but it is getting a bit blunt now I'm either getting a new blade or just a new guillotine Havnt decided yet
Its probably not the strength it says it it
It is actually
Decent
Honest opinion It's awful
Strange it crack The compression strength is only 16 same as NA Not that I'll ever be using it :rolleyes:
What you meant is "Its a crime not to prime"
Youd be better of having everything supplied by an independent retailer Then your only dealing with on party if theres any issues with anything
And the fact that NA flows like mud ;)
I know exactly what Ardex say about NA :confused:
Primer should always be used with every compound Theres no such thing as a best compound as such it is dependent on the subfloor as what is best...