Hi tarkett85, Are you able to advise on what smoothing compound you would recommend with a higher compression strength than Arditex NA please....
Thanks all for your replies. It seems there are a couple of things I did wrong. I wasn't aware of "live" vs "dead" adhesive and I didn't prime...
The bitumen wasn't hard and if I scrape it, it some residue sticks to my scraper.
Hi I have recently laid a parquet floor using in a herring bone pattern with a straight border. This is in an S shape hallway. As part of the...
Thanks guys, that's helped a lot. It's only one wall that's out and not by much so I'll make sure the border is the same width all the way round....
Hi I am laying oak parquet blocks in a herringbone pattern and I am going to have a border go around the outside in the form of two rows of...
Thanks for your prompt reply. I'll make sure I lay enough adhesive to give the coverage.
Hi I am planning to lay solid oak parquet blocks, 250 x 70 x 20. I have been sold Rewmar MS650 adhesive in the form of "sausages" that fit...